Figure 3. Comparison of temperature rise, thermal deformation, and laser-damage performance with and without water cooling. Cooling reduced the maximum surface temperature from 84.20 °C to 45.00 °C, lowered thermal-deformation PV from 12,292 nm to 3,082 nm, and increased the laser-induced damage threshold from 8,488 ± 127 W/cm2 to 13,581 ± 203 W/cm2.