Catalytic activity of Au₂₄Pt NCs-loaded CeO₂ and CeO₂ catalysts. CO oxidation profile of [Au₂₄Pt(PET)₁₈]⁰/CeO₂, [Au₂₄Pt(TBBT)₁₂(TDT)₃]⁰/CeO₂ and CeO₂ in the temperature range of 50-300 °C (a) without and (b) with oxidative pretreatment at 250 °C.