Figure 3 | Fracture surface after laser welding. (IMAGE)
Caption
Figure 3 | Fracture surface after laser welding. (a) 2-Burst, (b) 6-Burst, and (c) 8-Burst mode femtosecond laser welding. (i) SEM and (ii) BSE images of the fracture surface morphology on the metal surface of the joint. (iii) Post-melting surface features of the metal under spatial confinement.
Credit
Cong Wang et al.
Usage Restrictions
Credit must be given to the creator.
License
CC BY